  4. Influences of polymer concrete surfacing and localised load distribution on behaviour up to failure of an orthotropic FRP bridge deck
 
research article

Influences of polymer concrete surfacing and localised load distribution on behaviour up to failure of an orthotropic FRP bridge deck

Sebastian, W. M.
•
Keller, T.  
•
Ross, J.
2013
Composites Part B

This paper presents experimental results which demonstrate the important, but to date little-studied influence of surfacing on the response up to failure of orthotropic GFRP bridge decking local to concentrated loading. Four bonded deck specimens were tested, two without surfacing and two including a 30 mm thick polymer concrete surfacing layer. A specified steel plate-rubber pad ensemble which produced a load distribution generating high shear and low moment locally was used to load one surfaced and one unsurfaced specimen to failure, while a plate-pad system inducing modest shear and high moment locally (nearer the tyre effect) was used to fail the other two specimens. The surfaced specimens' load capacities exceeded those of their unsurfaced counterparts by 90% and 261% under the shear-dominant and moment-dominant loads respectively. For each surfaced specimen, failure occurred in part by formation of a distinctly curved crack in the polymer concrete. In contrast to reports of detached surfacing on real FRP deck bridges, no debonding was observed at the surfacing-deck interfaces during these tests. This suggests scope for significantly improved surfacing-deck bond integrity in practice. GFRP delamination, particularly within the directly loaded flange, also occurred in the four test specimens. The critical failure zone shifted from the flange's ends to its local midspan in changing from shear-dominant to moment-dominant loading. It is concluded that the status quo standard of testing unsurfaced deck specimens should be modified to testing of surfacing-deck systems. (c) 2012 Elsevier Ltd. All rights reserved.

  • Details
  • Metrics
Type
research article
DOI
10.1016/j.compositesb.2012.07.050
Web of Science ID

WOS:000314193200132

Author(s)
Sebastian, W. M.
Keller, T.  
Ross, J.
Date Issued

2013

Publisher

Elsevier

Published in
Composites Part B
Volume

45

Issue

1

Start page

1234

End page

1250

Subjects

Glass fibres

•

Delamination

•

Strength

•

Mechanical testing

•

FRP deck

Editorial or Peer reviewed

REVIEWED

Written at

EPFL

EPFL units
CCLAB  
Available on Infoscience
March 28, 2013
Use this identifier to reference this record
https://infoscience.epfl.ch/handle/20.500.14299/90822
Logo EPFL, École polytechnique fédérale de Lausanne
  • Contact
  • infoscience@epfl.ch

  • Follow us on Facebook
  • Follow us on Instagram
  • Follow us on LinkedIn
  • Follow us on X
  • Follow us on Youtube
AccessibilityLegal noticePrivacy policyCookie settingsEnd User AgreementGet helpFeedback

Infoscience is a service managed and provided by the Library and IT Services of EPFL. © EPFL, tous droits réservés