  4. Top-interface-controlled switching and fatigue endurance of (Pb, La)(Zr,Ti)O-3 ferroelectric capacitors
 
research article

Top-interface-controlled switching and fatigue endurance of (Pb, La)(Zr,Ti)O-3 ferroelectric capacitors

Stolichnov, I.  
•
Tagantsev, A.  
•
Setter, N.  
Show more
1999
Applied Physics Letters

Mechanisms of polarization switching and fatigue in (Pb, La)(Zr, Ti)O-3 (PLZT) films are studied by comparative analysis of degradation and leakage conduction of PLZT capacitors with Pt, SrRuO3 (SRO), and layered Pt/SRO (80/5 nm) electrodes. It is found that the asymmetrical Pt/SRO/PLZT/Pt structure exhibits a good fatigue performance in combination with low leakage like that on identically processed Pt/PLZT/Pt capacitor. This asymmetrical structure exhibits very unusual dependence of the endurance of switching polarization on the driving alternating-current (ac) electric field amplitude. Specifically, for high ac electric field amplitude it shows good switching endurance similar to SRO/PLZT/SRO capacitors, whereas for amplitude lower than 80 kV/cm a pronounced polarization fatigue similar to that of the conventional Pt/PLZT/Pt capacitors is observed. Based on the analysis of our results on fatigue and leakage conduction we conclude that: (i) In asymmetrical Pt/SRO/PLZT/Pt system the physical mechanisms of polarization switching vary depending on the driving voltage amplitude. The polarization switching endurance under high-amplitude cycling is governed only by the top SRO interface, whereas the degradation properties of the bottom Pt interface do not play any role. On the contrary, for driving voltage amplitudes lower than 80 kV/cm the bottom Pt-interface degradation is a limiting factor for the fatigue performance. (ii) The fatigue in PZT films is controlled by a mechanism related to the inhibition of near-by-electrode nucleation of opposite domains, as suggested earlier. (C) 1999 American Institute of Physics. [S0003-6951(99)04623-9].

  • Details
  • Metrics
Type
research article
DOI
10.1063/1.124158
Web of Science ID

WOS:000080519000042

Author(s)
Stolichnov, I.  
Tagantsev, A.  
Setter, N.  
Cross, J. S.
Tsukada, M.
Date Issued

1999

Published in
Applied Physics Letters
Volume

74

Issue

23

Start page

3552

End page

3554

Subjects

thin-films

•

electrodes

•

state

•

model

Note

Stolichnov, I Swiss Fed Inst Technol, Ceram Lab, CH-1015 Lausanne, Switzerland Swiss Fed Inst Technol, Ceram Lab, CH-1015 Lausanne, Switzerland Fujitsu Labs Ltd, Atsugi, Kanagawa 2430197, Japan

200BL

Cited References Count:13

Editorial or Peer reviewed

REVIEWED

Written at

EPFL

EPFL units
LC  
Available on Infoscience
August 21, 2006
Use this identifier to reference this record
https://infoscience.epfl.ch/handle/20.500.14299/233406
Logo EPFL, École polytechnique fédérale de Lausanne
  • Contact
  • infoscience@epfl.ch

  • Follow us on Facebook
  • Follow us on Instagram
  • Follow us on LinkedIn
  • Follow us on X
  • Follow us on Youtube
AccessibilityLegal noticePrivacy policyCookie settingsEnd User AgreementGet helpFeedback

Infoscience is a service managed and provided by the Library and IT Services of EPFL. © EPFL, tous droits réservés