  4. The effect of boundary conditions and sample aspect ratio on apparent d(33) piezoelectric coefficient determined by direct quasistatic method
 
research article

The effect of boundary conditions and sample aspect ratio on apparent d(33) piezoelectric coefficient determined by direct quasistatic method

Barzegar, A.  
•
Damjanovic, D.  
•
Setter, N.  
2004
Ieee Transactions on Ultrasonics Ferroelectrics and Frequency Control

The effect of boundary conditions (e.g., type of metal contacts) and sample geometry (e.g., sample aspect ratio) on measurements of direct longitudinal d(33) coefficient in piezoelectric ceramics is studied by direct quasistatic method. We show that at small aspect ratio (thickness/lateral dimension <0.1) the measured d(33meas) is as much as 30% lower than the true value, d(33true). Measured d(33) increases with increasing aspect ratio and reaches its true value at a threshold aspect ratio that is dependent on ceramic composition and is about approximate to0.5 in the case of soft and hard Pb(Zr,Ti)O-3. Experimental results show that, when the force is applied over the whole electroded surface of the sample, the d(33) depends only on the aspect ratio and not size of samples. The experimental results are compared with simulations using finite element modeling (FEM) and are interpreted in terms of distribution of strain/stress within the sample, which leads to functional dependence of the measured d(33) on transverse d(31) and shear d(15) coefficients. It is shown experimentally and by FEM that the value of d(33) at low aspect ratios depends on the type of metallic contacts used to collect the charge and apply the pressure on the sample. Effect of nonlinearity of the d(31) and d(15) coefficients on d(33) measurements also is considered.

  • Details
  • Metrics
Type
research article
DOI
10.1109/TUFFC.2004.1320781
Web of Science ID

WOS:000220779900001

Author(s)
Barzegar, A.  
Damjanovic, D.  
Setter, N.  
Date Issued

2004

Published in
Ieee Transactions on Ultrasonics Ferroelectrics and Frequency Control
Volume

51

Issue

3

Start page

262

End page

270

Subjects

thin-films

•

ceramics

•

nonlinearity

•

hysteresis

•

vibrations

•

disks

Note

Barzegar, A Swiss Fed Inst Technol, Sch Engn, Mat Inst, Ceram Lab, CH-1015 Lausanne, Switzerland Swiss Fed Inst Technol, Sch Engn, Mat Inst, Ceram Lab, CH-1015 Lausanne, Switzerland

811NZ

Cited References Count:24

Editorial or Peer reviewed

REVIEWED

Written at

EPFL

EPFL units
LC  
Available on Infoscience
August 21, 2006
Use this identifier to reference this record
https://infoscience.epfl.ch/handle/20.500.14299/233521
Logo EPFL, École polytechnique fédérale de Lausanne
  • Contact
  • infoscience@epfl.ch

  • Follow us on Facebook
  • Follow us on Instagram
  • Follow us on LinkedIn
  • Follow us on X
  • Follow us on Youtube
AccessibilityLegal noticePrivacy policyCookie settingsEnd User AgreementGet helpFeedback

Infoscience is a service managed and provided by the Library and IT Services of EPFL. © EPFL, tous droits réservés