Influence of heat treatment on the electrochemical behavior of nickel

The heat pretreatment of Ni at 500-700 Deg gives a nonstoichiometric Ni oxide which shows metallic cond. and low activity for O evolution; at higher temps. (>700 Deg), a nonconducting NiO (p-type semiconductor) is formed. [on SciFinder (R)]