Abstract

Diffuse scattering in the lead zirconate-titanate single crystal with a titanium concentration of 0.7 at % has been studied by the synchrotron radiation scattering method. Measurements have been performed both in the vicinity of the Brillouin zone center and at the M-point. Highly anisotropic diffuse scattering has been revealed in the paraelectric phase near the Brillouin zone center; diffuse scattering anisotropy is similar to that previously observed in pure lead zirconate. The temperature dependence of this diffuse scattering obeys a critical law with T (c) a parts per thousand 480 K. Diffuse scattering in the vicinity of the M-point weakly depends on temperature; this dependence behaves differently at M-points with various indices.