Continuous-wave four-wave mixing in cm-long Chalcogenide microstructured fiber

We present the experimental demonstration of broadband four-wave mixing in a 2.5 cm-long segment of AsSe Chalcogenide microstructured fiber. The parametric mixing was driven by a continuous-wave pump compatible with data signal wavelength conversion. Four-wave mixing products over more than 70 nm on the anti-stoke side of the pump were measured for 345 mW of pump power and 1.5 dBm of signal power. The ultrafast signal processing capability was verified through wavelength conversion of 1.4 ps pulses at 8 GHz repetition rate. (C) 2011 Optical Society of America


Published in:
Optics Express, 19, 621-627
Year:
2011
Publisher:
Optical Society of America
ISSN:
1094-4087