Performance polyamides built on a sustainable carbohydrate core
Sustainably producing plastics with performance properties across a variety of materials chemistries is a major challenge-especially considering that most performance materials use aromatic precursors that are still difficult to source sustainably. Here we demonstrate catalyst-free, melt polymerization of dimethyl glyoxylate xylose, a stabilized carbohydrate that can be synthesized from agricultural waste with 97% atom efficiency, into amorphous polyamides with performances comparable to fossil-based semi-aromatic alternatives. Despite the presence of a carbohydrate core, these materials retain their thermomechanical properties through multiple rounds of high-shear mechanical recycling and could be chemically recycled. Techno-economic and life-cycle analyses suggest selling prices close to those of nylon 66 with a reduction of global warming potential of up to 75%. This work illustrates the versatility of a carbohydrate moiety to impart performance that can compete with that of semi-aromatic polymers across two important materials chemistries.
document.pdf
Publisher's Version
http://purl.org/coar/version/c_970fb48d4fbd8a85
openaccess
CC BY
2.25 MB
Adobe PDF
902dd16817143039683667a0b3ccabd1