  4. Predicting Hot Tearing in Aluminium Castings
 
research article

Predicting Hot Tearing in Aluminium Castings

Drezet, Jean-Marie  
2000
Esaform Bulletin

In many casting processes, some stages, such as the starting phase in the direct chill casting of aluminium alloys, are particularly critical because of the propensity of some alloys to develop either hot tears which initiate at non zero liquid fraction, or cold cracks which nucleate and grow exclusively in the solid metal. Figure 1 shows a cracked rolling sheet ingot: two hot tears initiated during the starting phase of casting have grown up as the ingot was further cast. For some very sensitive alloys, up to 10 % of the ingots present some cracks and have to be remelted.

  • Files
  • Details
  • Metrics
Loading...
Thumbnail Image
Name

Drezet-Esaform-2000.PDF

Access type

openaccess

Size

415.79 KB

Format

Adobe PDF

Checksum (MD5)

973e4b85cb02075c642f01d09a29725a

Logo EPFL, École polytechnique fédérale de Lausanne
  • Contact
  • infoscience@epfl.ch

  • Follow us on Facebook
  • Follow us on Instagram
  • Follow us on LinkedIn
  • Follow us on X
  • Follow us on Youtube
AccessibilityLegal noticePrivacy policyCookie settingsEnd User AgreementGet helpFeedback

Infoscience is a service managed and provided by the Library and IT Services of EPFL. © EPFL, tous droits réservés